Mar 18, 2024 Læg en besked

ASTM A672 EFW Pipes

ASTM A672 standard specification for electric fusion welded steel pipe for high pressure service at moderate temperatures.

Chemical Requirements of ASTM A672 :

C P S
                 

ASTM A671, A672
-/A45 -/0.17 - 0.98 0.035 0.035 - A671/
A672
-/A50 -/0.22 -
CA55/A55 0.28 -
-/B55 -/0.20 0.13
~0.45
CB60/B60 0.24
CB65/B65 0.28
CB70/C70 0.31 1.30
-/C55 -/0.18 0.55
~0.98
CC60/C60 0.21
CC65/C65 0.24 0.79
~1.30
CC70/C70 0.27

Mechanical Properties of ASTM A672:

Welding point tensile strength (N/mm2)
Yield point (N/mm2) Tensile Stregth (N/mm2)
Pipes for pressure service ASTM A671, A672 -/A45 -/165 -/310~450 - -/30 -/310~450 A671/ A672
-/A50 -/185 -/345~485 -/28 -/345~485
CA55/A55 205 380~515 27 380~515
-/B55 -/205 -/380~515 -/27 -/380~515
CB60/B60 220 415~550 25 415~550
CB65/B65 240 450~585 23 450~585
CB70/B70 260 485~620 21 485~620
-/C55 -/205 -/380~515 -/27 -/380~515
CC60/C60 220 415~550 25 415~550
CC65/C65 240 450~585 23 450~585
CC70/C70 260 485~620 21 485~620

ASTM A672 EFW Pipes

Send forespørgsel

whatsapp

Telefon

E-mail

Undersøgelse